湿法烟气脱硫工程烟道膨胀节破裂的原因分析及处理
Cause Analysis and Treatment of Expansion Joint Crack of WFGD Projec

沈海涛,邓芙蓉
SHEN Hai-tao,DENG Fu-rong(Zhejiang Tiandi Environmental Protection Engineering Co.

摘要(Abstract):

某发电厂2台660 MW机组脱硫装置在投运后8个月内,GGH至吸收塔原烟道发生很大的整体位移,将吸收塔入口处的膨胀节拉裂,导致烟气泄漏。通过对烟道整体结构的分析,提出了相应的改进措施。实际运行情况证明改造合理有效。
The excessive displacement of the flue between GGH and absorber happened during eight months after FGD operation in 2×660 MW units of a power plant.The cracks appeared on the expansion joint at the absorber inlet that led to gas leakage.The treatment measure is put forward through the analysis of the whole flue structure.The actual operation after improvement indicates that the retrofit is reasonable and effective.

关键词(KeyWords): 湿法脱硫;烟道;膨胀节;破裂
WFGD;flue;expansion joint;crack

Abstract:

Keywords:

基金项目(Foundation):

作者(Author): 沈海涛,邓芙蓉
SHEN Hai-tao,DENG Fu-rong(Zhejiang Tiandi Environmental Protection Engineering Co.

DOI: 10.19585/j.zjdl.2013.08.014

扩展功能
本文信息
服务与反馈
本文关键词相关文章
本文作者相关文章
中国知网
分享